Title of article
Surface energetics of poly(N-vinyl-2-pyrrolidone)/chitosan blend films
Author/Authors
Tuncer C¸ aykara، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2006
Pages
6
From page
7430
To page
7435
Abstract
Poly(N-vinyl-2-pyrrolidone) (PVP) and chitosan (CTS) with three different molecular weights (MW: 150,000, 400,000 and
600,000 g/mol) blends were prepared as films having 13, 20, 33, 43 and 50% (w/w) CTS by solution casting method. Surface
properties of the films were analyzed by contact-angle measurements and scanning electron microscopy (SEM). The contact
angles of water, glycerol, ethylene glycol, formamide and paraffin oil drop were measured on these films. The contact-angle
results were evaluated in terms of surface free energy components by using Van Oss–Good methodology. It was found that all
PVP/CTS blend surfaces are enriched in low surface free energy component, i.e. CTS. This conclusion was further confirmed by
the cross-sectional SEM images observation of these blends.
Keywords
Chitosan , surface energy , blends , Contact angle
Journal title
Applied Surface Science