Title of article
Kinetics of hematite chlorination with Cl2 and Cl2 + O2: Part I. Chlorination with Cl2
Author/Authors
N. Kanari، نويسنده , , D. Mishra، نويسنده , , L. Filippov، نويسنده , , F. Diot، نويسنده , , J. Moch?n، نويسنده , , E. Allain، نويسنده ,
Issue Information
دوهفته نامه با شماره پیاپی سال 2010
Pages
8
From page
52
To page
59
Abstract
Preliminary tests of the chlorination of two iron oxides (wüstite and hematite) in various chlorinating gas mixtures were performed by thermogravimetric analysis (TGA) under non-isothermal conditions. Wüstite started to react with chlorine from about 200 °C generating ferric chloride and hematite as the final reaction products. The presence of a reducing and oxidizing agent in the chlorinating gas mixtures influenced the chlorination reactions of both iron oxides, during non-isothermal treatment, only at temperatures higher than 500 °C.
The chlorination kinetics of hematite with Cl2 have been studied in details between 600 and 1025 °C under isothermal chlorination. The values of the apparent activation energy (Ea) were about 180 and 75 kJ/mol in the temperature ranges of 600–875 and 875–1025 °C, respectively. The apparent reaction order with respect to Cl2 was found to be 0.67 at 750 °C. Mathematical model fitting of the kinetics data was carried out to determine the most probable reaction mechanisms.
Keywords
Hematite , Thermogravimetric analysis , kinetics , Chlorination