• Title of article

    Heat capacity, enthalpy and entropy of SrBi2O4 and Sr2Bi2O5

  • Author/Authors

    J. Leitner، نويسنده , , D. Sedmidubsk?، نويسنده , , K. Ruzicka and V. V. Diky ، نويسنده , , P. Svoboda، نويسنده ,

  • Issue Information
    دوهفته نامه با شماره پیاپی سال 2012
  • Pages
    6
  • From page
    60
  • To page
    65
  • Abstract
    Heat capacity and enthalpy increments of ternary strontium bismuth(III) oxides SrBi2O4 and Sr2Bi2O5 were measured by the relaxation time method (2–210 K), DSC (253–352 K) and drop calorimetry (570–1072 K). Temperature dependencies of the molar heat capacity in the form Cpm = 161.97 + 45.936 × 10−3 T – 1.7862 × 106/T2 J K−1 mol−1 and Cpm = 197.48 + 87.463 × 10−3 T – 1.9282 × 106/T2 J K−1 mol−1 for SrBi2O4 and Sr2Bi2O5, respectively, were derived by the least-squares method from the experimental data. The molar entropies at 298.15 K, S°m(298.15 K) = 206.1 ± 1.1 J K−1 mol−1 for SrBi2O4 and S°m(298.15 K) = 261.2 ± 1.4 J K−1 mol−1 for Sr2Bi2O5, were evaluated from the low temperature heat capacity measurements.
  • Keywords
    Heat capacity , Enthalpy increments , Strontium bismuth(III) oxides , Calorimetry , Entropy
  • Journal title
    Thermochimica Acta
  • Serial Year
    2012
  • Journal title
    Thermochimica Acta
  • Record number

    1199959