Abstract
BaTiO3 (BT) powders were synthesized by the hydrothermal method for fabricating lead-free barium titanate piezoelectric ceramics. The obtained powders were washed by distilled water and 0.01N acetic acid solutions separately, and utilized to obtain piezoelectric ceramics by traditional sintering. BT ceramics with the highest piezoelectric properties (d33 value is over 190 pC/N) was obtained from the BT powder synthesized at 250 °C and washed by acetic acid solution. The influence of washing method and sintering temperature on the piezoelectric properties of BT ceramics were studied. The reasons were investigated by comparing the properties of BT powders and their compacts sintered at different temperature.
Keywords
A. Powders: chemical preparation , D. BaTiO3 , C. Piezoelectric properties , lead-free
Journal title
Ceramics International
Serial Year
2009
Journal title
Ceramics International
Record number
1271621
Link To Document