Attrition characteristics and mechanisms for limestone particles in an air-jet apparatus
Author/Authors
Xiao، نويسنده , , Gang and Grace، نويسنده , , John R. and Lim، نويسنده , , C. Jim، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2011
Pages
9
From page
183
To page
191
Abstract
Attrition is very important for limestone particles used to capture SO2 and CO2. In this study, the attrition of limestone particles was investigated at room temperature using an air-jet apparatus, based on the standard ASTM D 5757-00 method. The mass percent of fines increased almost linearly with time for 125–850 μm particles. In the attrition process, abrasion was initially the main mode of attrition for 710–850 μm particles, causing the particles to become rounded and smooth. Fragmentation became important as well when the particles reached the 200–400 μm range and became the main mode of attrition for particles smaller than 180 μm. The change in the mode of attrition is important, as attrition models tend to assume that the mode is always the same.
Keywords
Attrition , Air Jets , Limestone , fragmentation , Abrasion
Journal title
Powder Technology
Serial Year
2011
Journal title
Powder Technology
Record number
1694668
Link To Document