Title of article
A higher conductivity Bi2O3-based electrolyte
Author/Authors
Jiang، نويسنده , , Naixiong and Wachsman، نويسنده , , Eric D and Jung، نويسنده , , Su-Ho، نويسنده ,
Issue Information
هفته نامه با شماره پیاپی سال 2002
Pages
7
From page
347
To page
353
Abstract
We have developed a Bi2O3 electrolyte doped with Dy2O3 and WO3 (DyWSB) that exhibits a higher conductivity than that of 20 mol% erbia stabilized bismuth oxide (20ESB), thus, giving it the highest conductivity of any known solid oxide electrolyte. Electrical conductivity results of the Dy–W stabilized bismuth oxide system are presented. The dopants were selected based on their polarizability and its effect on structural stability and conductivity. At 800 °C, the conductivity of (BiO1.5)0.88(DyO1.5)0.08(WO3)0.04 is 0.57 S/cm (1.5 times as high as that of 20ESB), and at 500 °C, the conductivity is 0.043 S/cm (2 times as high as that of 20ESB).
Keywords
polarizability , Double doping , structural stability , Bismuth oxide , electrical conductivity
Journal title
Solid State Ionics
Serial Year
2002
Journal title
Solid State Ionics
Record number
1714542
Link To Document