• Title of article

    TSDC and dielectric properties of Nd-doped KGd(WO4)2 crystals

  • Author/Authors

    Andriyevsky، نويسنده , , B and Patryn، نويسنده , , A and Czapla، نويسنده , , Z and Dacko، نويسنده , , S، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2004
  • Pages
    5
  • From page
    246
  • To page
    250
  • Abstract
    Temperature dependencies of the thermally stimulated depolarization current (TSDC) and the dielectric properties at alternating current have been measured for Nd-doped KGd(WO4)2 crystal in the range of 250–400 K. The corresponding activation energy calculated in the range of 330–400 K is equal to 0.75±0.05 eV. Small maximum in TSDC spectrum at 330 K, characterizing by the activation energy 1.68±0.20 eV can be connected with small structural defects associated with doped Nd3+ ions. Reversible character of the anomaly on the temperature dependence of dielectric permittivity ε(T) at 330 K shows that the weak structure transformation of the phase transition type can take place in the crystal.
  • Keywords
    Nd:KGd(WO4)2 crystal , Thermally stimulated depolarization current , dielectric properties , Phase transitions
  • Journal title
    MATERIALS SCIENCE & ENGINEERING: B
  • Serial Year
    2004
  • Journal title
    MATERIALS SCIENCE & ENGINEERING: B
  • Record number

    2140949