Title of article
Brittle failure of Alloy 693 at elevated temperatures
Author/Authors
Singh، نويسنده , , Jung B. and Verma، نويسنده , , A. and Thota، نويسنده , , Manoj K. and Chakravartty، نويسنده , , J.K.، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2014
Pages
5
From page
88
To page
92
Abstract
This reports transgranular brittle failure during high temperature deformation of a wrought Alloy 693 received in solution annealed condition. This has been attributed to the inability to suppress the formation of γ′ precipitates during quenching after the solution annealing treatment. The fine γ′ precipitates severely strained the matrix and inhibited plasticity during subsequent deformation.
Keywords
diagram , Continuous cooling transformation (CCT) , Brittle failure , Alloy 693 , ?? precipitates , High temperature deformation