• Title of article

    Joining dental ceramic layers with glass

  • Author/Authors

    Saied، نويسنده , , M.A. and Lloyd، نويسنده , , I.K. and Haller، نويسنده , , W.K. and Lawn، نويسنده , , B.R.، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2011
  • Pages
    6
  • From page
    1011
  • To page
    1016
  • Abstract
    Objective he hypothesis that glass-bonding of free-form veneer and core ceramic layers can produce robust interfaces, chemically durable and esthetic in appearance and, above all, resistant to delamination. s of independently produced porcelains (NobelRondo™ Press porcelain, Nobel BioCare AB and Sagkura Interaction porcelain, Elephant Dental) and matching alumina or zirconia core ceramics (Procera alumina, Nobel BioCare AB, BioZyram yttria stabilized tetragonal zirconia polycrystal, Cyrtina Dental) were joined with designed glasses, tailored to match thermal expansion coefficients of the components and free of toxic elements. Scanning electron microprobe analysis was used to characterize the chemistry of the joined interfaces, specifically to confirm interdiffusion of ions. Vickers indentations were used to drive controlled corner cracks into the glass interlayers to evaluate the toughness of the interfaces. s ass-bonded interfaces were found to have robust integrity relative to interfaces fused without glass, or those fused with a resin-based adhesive. icance ructural integrity of the interfaces between porcelain veneers and alumina or zirconia cores is a critical factor in the longevity of all-ceramic dental crowns and fixed dental prostheses.
  • Keywords
    Crown , Glass bonding , Interface , Veneer , Ceramic core
  • Journal title
    Dental Materials
  • Serial Year
    2011
  • Journal title
    Dental Materials
  • Record number

    2317777