Title of article
Relationship between fracture toughness and porosity of clay brick panels used in ventilated façades: Initial investigation
Author/Authors
D’Orazio، نويسنده , , Marco and Lenci، نويسنده , , Stefano and Graziani، نويسنده , , Lorenzo، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2014
Pages
14
From page
108
To page
121
Abstract
Fired clay elements are commonly used for external cladding, but the fragility of this material causes crack formation that, in conjunction with environmental actions, can even break clay brick elements. In order to optimize this technology, a relationship between fracture toughness and porosity can be helpful.
s paper, linear elastic fracture mechanics (LEFM) was applied to study the fragility of clay bricks used in ventilated façades. Stress intensity factor KIC was calculated under Mode I (opening mode) loading condition. Pore structure was evaluated by digital image analysis (DIA). We found that an increase of about 200 μm2 in pore dimension corresponds to a decrease in fracture toughness of about 24%.
Keywords
porosity , Porous structure , Stress intensity factor , fracture toughness , Ventilated façades