Title of article
Late degradation tissue response to poly(Image -lactide) bone plates and screws
Author/Authors
J. E. Bergsma، نويسنده , , W. C. De Bruijn، نويسنده , , F. R. Rozema، نويسنده , , R. R. M. Bos، نويسنده , , G. Boering، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 1995
Pages
7
From page
25
To page
31
Abstract
Patients with fractures of the zygomatic bone were treated with high molecular weight poly(Image -lactic) acid (PLLA) bone plates and screws. Three years after implantation four patients returned to our department with a swelling at the site of implantation. At the recall of the remaining patients we found an identical type of swelling after the same implantation period. To investigate the nature of the tissue reaction, eight patients were reoperated for the removal of the swelling. The implantation period of the PLLA material varied from 3.3 to 5.7 years. Microscopic evaluation and molecular weight measurements were performed. The excised material showed remnants of degraded PLLA material surrounded by a dense fibrous capsule. Ultrastructural investigation showed crystal-like PLLA material internalized by various cells. The results of this investigation suggest that the PLLA material slowly degrades into particles with a high crystallinity. The intra- and extracellular degradation rate of these particles is very low. After 5.7 years of implantation, these particles were still not fully resorbed.
Keywords
Enzyme activity , biodegradation , Tissue response , Poly (Image -lactide)
Journal title
Biomaterials
Serial Year
1995
Journal title
Biomaterials
Record number
542171
Link To Document