Abstract
This work presents a systematic investigation of the influence of time and temperature in
the sensitization of stainless steel AISI 304L, AISI 316L, AISI 321 and AISI 347 pipes used in
petroleum refining plants. The sensitization was assessed by Scanning Electron
Microscopy (SEM) according to ASTM A-262 and by the Double Loop Electrochemical
Potentiokinetic Reactivation test (DLEPR). The results showed that all steels did not present
sensitization at operating temperature (380◦C) in the desulfurizers process, but the
temperature of 500◦C was critical to the appearing of sensitization for the both low carbon
stainless steels and AISI 321 SS, while for the AISI 347 the critical temperature was 550◦C.
The stabilized steels confirmed to be more resistant to sensitization than the low carbon
stainless steels, and niobium showed to be more efficient stabilizing agent than titanium.
C 2005 Springer Science + Business Media, Inc
Journal title
Journal of Materials Science
Serial Year
2005
Journal title
Journal of Materials Science
Record number
829443
Link To Document