Title of article :
Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m
Author/Authors :
J.P Viricelle، نويسنده , , P Goursat، نويسنده , , D Bahloul-Hourlier، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2001
Pages :
8
From page :
607
To page :
614
Abstract :
The oxidation behaviour of a 2.5D multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m was investigated in a dry atmosphere O2 (20 vol.%) CO2 (5 vol.%) He and in the presence of water vapour H2O (2.3 vol.%). The matrix denoted (SiBC)m is constituted of three phases: silicon carbide, boron carbide and a SiBC phase. The aim of boron incorporation is to improve the oxidation resistance of the composite by boron oxide or borosilicate formation. The transformations were followed by thermogravimetry during isothermal experiments of 20 h exposure in the range 600–1200°C and the changes of the specific area of the samples were measured by krypton adsorption at 77 K. The results of this study show that effective protection occurs in the range 650–900°C and is mainly related to the oxidation of boron carbide. At higher temperatures, boron oxide is no longer protective because of its volatilisation and consumption by reaction with water vapour. However, the two other constituents of the matrix, SiC and SiBC, lead to self-healing behaviour by both borosilicate and silica formation.
Keywords :
Ceramic-matrix composite , Oxidation
Journal title :
COMPOSITES SCIENCE AND TECHNOLOGY
Serial Year :
2001
Journal title :
COMPOSITES SCIENCE AND TECHNOLOGY
Record number :
1039370
Link To Document :
بازگشت