Title of article :
Simple oxalate precursor route for the preparation of brain-like shaped barium–strontium titanate: Ba0.6Sr0.4TiO3
Author/Authors :
Mingli Li، نويسنده , , Hui Liang، نويسنده , , Mingxia Xu، نويسنده ,
Issue Information :
دوهفته نامه با شماره پیاپی سال 2008
Pages :
5
From page :
337
To page :
341
Abstract :
Through adding quantitative ammonia into a precursor solution containing stoichiometric quantities of Ba and Sr ions before the co-precipitation procedure, a simple oxalate co-precipitation method based one-step cation-exchange reaction between the stoichiometric solutions of oxalotitanic acid (HTO) and barium + strontium nitrate is investigated successfully for the quantitative precipitation of barium–strontium titanyl oxalate (BSTO): Ba0.6Sr0.4TiO(C2O4)2·4H2O precursor powders. The pyrolysis of BSTO at 800 °C/4 h in air produced the homogeneous brain-like shaped barium–strontium titanate (Ba0.6Sr0.4TiO3: BST) powders. The characterization studies were carried on the as-dried BSTO and calcined BST powders by various physicochemical techniques, IR, DSC/TGA, XRD, SEM, etc. It revealed that the BST powders are cubic, stoichiometric, highly pure, sub-micron-sized with nearly uniform size, brain-like shape and agglomerated nature.
Keywords :
Grazing incidence X-ray diffraction , Ceramics , Microstructure , Chemical synthesis
Journal title :
Materials Chemistry and Physics
Serial Year :
2008
Journal title :
Materials Chemistry and Physics
Record number :
1066285
Link To Document :
بازگشت