    High thermal stability of SAPO-40 in n-octane cracking Original Research Article

  • Author/Authors

    Miroslaw Derewinski، نويسنده , , Denise Barthomeuf، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 1995
  • Pages
    10
  • From page
    79
  • To page
    88
  • Abstract
    SAPO-40 is a highly active and thermally stable cracking catalyst. A comparison with LZY-82 and SAPO-37 in n-octane cracking shows that after pretreatment at around 800°C and above it is more active than LZY-82. Upon pretreatment at increasing temperature its hydrogen transfer activity decreases while that of SAPO-37 increases. The results are related to the unusually thin SAPO-40 crystals and to the distribution of silicon atoms in the framework.
  • Keywords
    Cracking , n-Octane , SAPO-40 , Stability (thermal) , Zeolites