Silicon nitride ceramics with Y2O3 and Al2O3 as sintering additives were corroded in 1 N sulphuric acid at 90 °C. Any classical corrosion rate model cannot describe the overall kinetics of the corrosion process successfully. At longer corrosions times a kinetic break occurs, after which slow linear corrosion kinetics prevail. The passivation is due to the formation of a defective silica sub-layer in the corrosion zone. We show that it is possible to enforce this passivation long before it would occur naturally by a simple hot drying (150 °C) procedure after a critical time. As consequence the total mass loss decreases by a factor of 2–3.
Keywords :
C. Corrosion , D. Si3N4 , E. Structural applications , B. Grain boundary
Journal title :
Ceramics International
Journal title :
Ceramics International