• Title of article

    Helium release and diffusion mechanism in SiC containing B4C

  • Author/Authors

    Bambang Pramono، نويسنده , , Yudi and Yano، نويسنده , , Toyohiko، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2004
  • Pages
    5
  • From page
    1170
  • To page
    1174
  • Abstract
    Helium release measurement have been carried out in the temperature range of 750–1260 °C for neutron-irradiated α-SiC powder. The powders were obtained from SiC ceramics containing B4C with varying contents of 10B, i.e., 4.2 × 1016, 1.13 × 1017 and 1.84 × 1017 atom/mg. Neutron irradiation was conducted up to a fluence of 2.8 × 1024 n/m2 (E>0.1 MeV) at ∼300 °C. The diffusion coefficients were calculated for the temperature region of 750–1060 °C and for time intervals 0–10, 10–60 min and 1–6 h at each temperature. The diffusion coefficient of He for SiC was affected by the original 10B concentration. Both helium diffusion coefficient and apparent activation energy were smaller for higher concentrations of 10B.
  • Journal title
    Journal of Nuclear Materials
  • Serial Year
    2004
  • Journal title
    Journal of Nuclear Materials
  • Record number