Title of article :
Deuterium and helium retentions of V–4Cr–4Ti alloy used as first wall of breeding blanket in a fusion reactor
Author/Authors :
Hirohata، نويسنده , , Yuko and Yamada، نويسنده , , Tsuyoshi and Yamauchi، نويسنده , , Yuji and Hino، نويسنده , , Tomoaki and Nagasaka، نويسنده , , Takuya and Muroga، نويسنده , , Takeo، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2006
Pages :
7
From page :
33
To page :
39
Abstract :
The deuterium and helium retention properties of V–4Cr–4Ti alloy were investigated by thermal desorption spectroscopy (TDS). Ion energies of deuterium and helium were taken at 1.7 and 5 keV, respectively. The retained amount of deuterium in the sample irradiated at 380 K increased with the ion fluence and was not saturated to fluence of up to 1 × 1023 D/m2. For the irradiation at 773 K, 0.1% of implanted deuterium was retained at the highest fluence. For the helium ion irradiation at room temperature, three groups of desorption peaks appeared at around 500, 850, and 1200 K in the TDS spectrum. In the lower fluence region (<1 × 1021 He/m2), the retained helium desorbed mainly at around 1200 K. With increasing fluence, the amount desorbed at 500 K increased. Total amount of retained helium in the samples saturated at fluence up to 5 × 1021 He/m2 and saturation level was 2.7 × 1021 He/m2.
Journal title :
Journal of Nuclear Materials
Serial Year :
2006
Journal title :
Journal of Nuclear Materials
Record number :
1362992
Link To Document :
بازگشت