Title of article :
Toughening enhanced at elevated temperatures in an alumina/zirconia dual-phase matrix composite reinforced with silicon carbide whiskers
Author/Authors :
Akatsu، نويسنده , , Takashi and Nakanishi، نويسنده , , Shin-ichi Tanabe، نويسنده , , Yasuhiro and Wakai، نويسنده , , Fumihiro and Yasuda، نويسنده , , Eiichi، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2013
Pages :
7
From page :
3157
To page :
3163
Abstract :
A unique temperature dependence of toughening is observed in an alumina/zirconia dual-phase matrix composite reinforced with silicon carbide whiskers. The work of fracture (WOF) of the composite is maximized at 400 °C to 130 J/m2, which is about 6.5 times larger than that of monolithic alumina at room temperature. The WOF decreases sharply with an increase in temperature above 400 °C. The enhanced toughening at elevated temperatures is described by the stress-induced transformation toughening of tetragonal zirconia, which is affected by the internal thermal stress owing to thermoelastic mismatch between the matrix and the whiskers. The maximum WOF is not given only by the stress-induced transformation but also by the crack-face bridging of the whiskers. The WOF was optimized at a specific zirconia volume fraction of 0.7 in the matrix, which was essentially due to the maximized tensile internal stress on zirconia in the dual-phase matrix.
Keywords :
ZrO2 , Al2O3 , SiC whiskers , Work of fracture , elevated temperatures
Journal title :
Journal of the European Ceramic Society
Serial Year :
2013
Journal title :
Journal of the European Ceramic Society
Record number :
1415803
Link To Document :
بازگشت