Title of article :
Characteristic energy band values and electron attenuation length of a chemical-vapor-deposition diamond (0 0 1)2 × 1 surface
Author/Authors :
Kono، نويسنده , , S. and Saitou، نويسنده , , T. and Kawata، نويسنده , , H. and Goto، نويسنده , , T. and Kakefuda، نويسنده , , Y. and Komeda، نويسنده , , T.، نويسنده ,
Issue Information :
هفته نامه با شماره پیاپی سال 2009
Abstract :
The characteristic energy band values such as the Fermi-level position with respect to valence band top for a boron-doped p-type hydrogen-terminated chemical-vapor-deposition (CVD) diamond (0 0 1)2 × 1 surface and for a clean CVD diamond (0 0 1)2 × 1 surface have been determined by a new method with an accuracy of ±0.02 eV. The electron attenuation length for the clean diamond (0 0 1)2 × 1 surface for the electron kinetic energy of C 1s X-ray photoemission peak by Mg Kα excitation is experimentally determined to be 2.1–2.2 nm. These values are compared and discussed with the previously reported experimental and simulation values.
Keywords :
Chemical-vapor-deposition , Electron attenuation length , Characteristic surface energy band values , diamond , Surface Fermi-level , (0 , 1)2 , 1 Surface , × , 0