Title of article :
Ion dynamics in mechanochemically synthesized amorphous fast ionic conductor Ag2S–Sb2S3
Author/Authors :
Tiwari، نويسنده , , J.P. and Shahi، نويسنده , , K.، نويسنده ,
Issue Information :
هفته نامه با شماره پیاپی سال 2005
Pages :
10
From page :
1271
To page :
1280
Abstract :
Frequency dependent electrical conductivity (σ′) of mechanochemically synthesized amorphous fast ion conductors (FICs) xAg2S–Sb2S3 (x=70, 80, 85) is investigated in the frequency range 5 Hz–13 MHz and temperature range 95–385 K. While the universal dynamic response (UDR) model, σ′ (ω)=σdc(T)+A(T)ωn, does reproduce the shape of σ′ (ω) spectra, the σdc(T) and A(T) show anomalous characteristics. Both exhibit two distinct Arrhenius regions, a low temperature region with a lower value of activation energy (E) and a high temperature region with higher value of activation energy. Further the frequency exponent n is a (decreasing) function of temperature, decreasing slowly at lower temperatures but more rapidly at higher temperatures. The correlation Eac=(1−n)Edc appears satisfactory in the low temperature region but unsatisfactory at higher temperatures. The isochronal representation of ac conductivity, σ′ vs. 1000/T at different frequencies, reveals the existence of a third regime, which is currently under active discussion and is known as superlinear power law (SLPL).
Keywords :
mechanochemistry , Frequency dependent conductivity , Amorphous electrolytes , Power law behaviour of the ac conductivity , Ball-milling
Journal title :
Solid State Ionics
Serial Year :
2005
Journal title :
Solid State Ionics
Record number :
1717751
Link To Document :
بازگشت