Author/Authors :
Ke، نويسنده , , Shanming and Huang، نويسنده , , Haitao and Fan، نويسنده , , Huiqing and Chan، نويسنده , , H.L.W. and Zhou، نويسنده , , L.M.، نويسنده ,
Abstract :
Ba0.6Sr0.4TiO3–MgTiO3 (BST–MT) composite ceramics were prepared by reaction of BST powders with molten MgCl2. The sintered composites exhibit a five orders of magnitude decrease in the dc resistivity as the relative humidity (RH) was increased from 5 to 92%. The ac conductivity of the samples obeys a power law at different temperatures within the frequency range of 10 Hz to 10 MHz.
Keywords :
BST , Ferroelectrics , Conductivity , Humidity sensor