• Title of article

    A new material for hip prosthesis without considerable debris release

  • Author/Authors

    Franco Borruto، نويسنده , , Adelina، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 2010
  • Pages
    6
  • From page
    908
  • To page
    913
  • Abstract
    This work presents an alternative bearing surface in the field of total hip replacements. It is composed of a polymer composite polyether-ether-ketone (Peek) as the matrix and a carbon fibre as reinforcement. thors carried out experimental research in order to investigate the formation of debris caused by tribological coupling of three types of Peek and cobalt chrome alloy. ar tests (ASTM 99G) have been performed with a pin on disc tribometer in an air environment, under the following conditions: dry, water lubrication using demineralised water as a lubricant and human serum. od of filtering under vacuum is used to extract the debris from the lubricants used in the tribological test, and the analysis at Scanning Electron Microscopy (SEM) is used to characterize the debris.
  • Keywords
    Hip , Debris , WEAR , Carbon fibre Peek
  • Journal title
    Medical Engineering and Physics
  • Serial Year
    2010
  • Journal title
    Medical Engineering and Physics
  • Record number

    1731066