Melt fracture of HDPEs: Metallocene versus Ziegler–Natta and broad MWD effects
Author/Authors :
Ansari ، نويسنده , , Mahmoud and Inn، نويسنده , , Yong W. and Sukhadia، نويسنده , , Ashish M. and DesLauriers، نويسنده , , Paul J. and Hatzikiriakos، نويسنده , , Savvas G.، نويسنده ,
Issue Information :
دوهفته نامه با شماره پیاپی سال 2012
Pages :
7
From page :
4195
To page :
4201
Abstract :
The melt fracture of high-density polyethylenes (HDPEs) is studied primarily as a function of molecular weight and its distribution for broad molecular weight distribution metallocene and Ziegler–Natta catalyst resins. It is found that sharkskin and other melt fracture phenomena are very different for these two classes of polymers, although their rheological behaviors are nearly the same for many of these. Moreover, the metallocene HDPE shows significant slip at the die wall without exhibiting stick-slip transition. Important correlations are derived between the critical conditions for the onset of melt fracture and molecular characteristics.
Keywords :
Broad molecular weight distribution , Extrusion instabilities , Stick-slip