Author/Authors :
Ci، نويسنده , , Lijie and Xie، نويسنده , , Sishen and Tang، نويسنده , , Dongsheng and Yan، نويسنده , , Xiaoqin and Li، نويسنده , , Yubao and Liu، نويسنده , , Zuqin and Zou، نويسنده , , Xiaoping and Zhou، نويسنده , , Weiya and Wang، نويسنده , , Gang، نويسنده ,
Abstract :
Single wall carbon nanotubes (SWNTs) without amorphous carbon coating were prepared by thermally decomposing acetylene (C2H2) at the temperature range 750–1200 °C in a floating iron catalyst system. The C2H2 partial pressure was controlled to make a carbon supply limiting growth of SWNTs. The higher reaction temperature above 1100 °C seemed not to favor the SWNT production due to the quick thermal decomposition of C2H2.