Title of article :
The characterization of borided pure tungsten
Author/Authors :
Usta، نويسنده , , M. and Ozbek، نويسنده , , I. Yilmaz-Ipek، نويسنده , , M. and Bindal، نويسنده , , C. and Ucisik، نويسنده , , A.H.، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2005
Pages :
5
From page :
330
To page :
334
Abstract :
This study reports on mechanical properties of borided pure tungsten. Boronizing heat treatment was performed in a solid medium consisting of Ekabor powders at 940 °C for 2, 4, and 8 h. The presence of WB on the surface of pure tungsten was confirmed by XRD analysis. Metallographic studies revealed an almost uniform and compact boride layer on the surface of the pure tungsten. The thickness of boride layer ranged from 10 to 42 μm with some scatters. The hardness of borided specimens decreased with the distance from the surface to the interior of the test material. The hardness of the boride on the substrate was 2500 HV while the hardness of the substrate was 445 HV.
Keywords :
Boronizing , Hardness , Tungsten boride , borides , Tungsten
Journal title :
Surface and Coatings Technology
Serial Year :
2005
Journal title :
Surface and Coatings Technology
Record number :
1809423
Link To Document :
بازگشت