Abstract :
Novel quaternary Ti–Si–C–N coatings composed of nanocrystalline Ti(C, N), amorphous phases of Si3N4 and C, and occasionally free Si and nanocrystalline TiSi2 were deposited on high-speed steel (HSS) substrate at 550 °C using pulsed d.c. plasma chemical vapor deposition (PCVD) technique from TiCl4, SiCl4, CH4, N2, H2 and Ar mixtures. It was found that the hardness increased with the increase of C content and reached the maximum value of approximately 48 GPa at the C content of 38.6 at.%. However, the crystallite size decreased to a minimum value of approximately 7 nm at the content of 38.6 at.% C. It could be detected that crystallite size and hardness almost remained stable during annealing up to 900 °C for Ti–Si–C–N coatings. However, a sharp decrease in the hardness was observed after annealing at 1000 °C due to the growth of grain. A shift of the diffraction peaks was towards higher 2θ for Ti–Si–C–N coatings after annealing at increasing temperatures because of evaporation of COx and resultant loss of C from coating at elevated temperature. In addition, SiOx, TiOx were detected in Ti–Si–C–N coatings after annealing at 1100 °C.
Keywords :
Super hard Ti–Si–C–N nanocomposite coatings , PCVD , Microhardness , Annealing , Crystallite size
Journal title :
Surface and Coatings Technology
Journal title :
Surface and Coatings Technology