• Title of article

    Influence of tungsten and rhenium concentration on creep properties of a second generation superalloy

  • Author/Authors

    Wِllmer، نويسنده , , S and Mack، نويسنده , , T and Glatzel، نويسنده , , U، نويسنده ,

  • Pages
    4
  • From page
    792
  • To page
    795
  • Abstract
    Creep properties at three different temperatures (1123, 1253 and 1373 K) for five single crystal alloys with varying Re and W content are presented. Tungsten content has been varied between 3.0 and 3.6 wt.%, rhenium between 2.3 and 2.9 wt.%. Creep properties, such as minimum creep rate, time to reach 1, or 2% strain and time to failure have been evaluated. For the low temperature regime, two parts of rhenium can be replaced by one part of tungsten. In the intermediate range, the ratio cW/cRe≈1.3 has to be fulfilled with the constraint that cRe≥2.3 wt.%. At high temperature the sum of W plus Re concentration determines the time to failure.
  • Keywords
    Superalloy , alloy design , rhenium , creep strength
  • Journal title
    Astroparticle Physics
  • Record number

    2059658