Abstract :
A significant amount of research has been generated on improving the properties of β-tricalcium phosphate (TCP). The sintering behavior of β-TCP, the resulting microstructure and properties are strongly influenced by several factors as, for example, the processing method, the presence of additives (MgO, SiO2, Li2O, Al2O3) and the presence of α and β crystal structures. The aim of this work was to study the effect of addition of MnO2 on sintering behavior, physical properties and microstructure of tricalcium phosphate (TCP). Powder mixtures of TCP with a fixed concentration of 5 wt.% MnO2 were either pressureless sintered or hot-pressed at 1200 or 1250 °C for 1 h. The results obtained (X-ray diffraction, firing shrinkage, porosity and density) explain the effect that addition of MnO2 and sintering processing have on the properties of β-TCP. sults showed that the incorporation of 5 wt.% MnO2 has improved the densification process of the TCP matrix.
Keywords :
Tricalcium phosphate , manganese oxide , Sintering , mechanical properties
Journal title :
Materials Science and Engineering C
Serial Year :
2008
Journal title :
Materials Science and Engineering C
Record number :
2096742
Link To Document :
بازگشت