Title of article :
Spark plasma sintered Al2O3–YSZ–TiO2 composites: Processing, characterization and in vivo evaluation
Author/Authors :
Ormanci، نويسنده , , Ozden and Akin، نويسنده , , Ipek and Sahin، نويسنده , , Filiz and Yucel، نويسنده , , Onuralp and Simon، نويسنده , , Viorica and Cavalu، نويسنده , , Simona and Goller، نويسنده , , Gultekin، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2014
Abstract :
Al2O3 and Al2O3–YSZ composites containing 3 and 5 wt.% TiO2 were prepared by spark plasma sintering at temperatures of 1350–1400 °C for 300 s under a pressure of 40 MPa. The grain growth of alumina was suppressed by the addition of YSZ. Al2O3–YSZ composites showed higher hardness than monolithic Al2O3. There was not a considerable difference in hardness values for Al2O3–YSZ composites containing 10 and 20 vol.% YSZ and the addition of TiO2 decreased the hardness of the composites. The fracture toughness of Al2O3 increased from 2.8 MPa·m1/2 to 4.3 MPa·m1/2 with the addition of 10 vol.% YSZ, further addition resulted in higher fracture toughness values. The fracture toughness values were increased with TiO2 addition and the highest value of fracture toughness, 5.3 MPa·m1/2, was achieved with the addition of 20 vol.% YSZ and 5 wt.% TiO2. Preliminary in vivo tests demonstrated the biocompatibility and osseointegration of the composites after 6 week post-implantation in femur of Wistar rats.
Keywords :
In vivo evaluation , Al2O3 , spark plasma sintering , YSZ , TIO2
Journal title :
Materials Science and Engineering C
Journal title :