• Title of article

    Microstructure and mechanical properties of a Mg-4Y-3RE alloy processed by thermo-mechanical treatment

  • Author/Authors

    Mohri، نويسنده , , Takeshi and Mabuchi، نويسنده , , Mamoru and Saito، نويسنده , , Naobumi and Nakamura، نويسنده , , Mamoru، نويسنده ,

  • Issue Information
    روزنامه با شماره پیاپی سال 1998
  • Pages
    8
  • From page
    287
  • To page
    294
  • Abstract
    Thermo-mechanical treatments consisting of hot extrusion at 573 or 673 K and artificial aging at 473 K were carried out on a Mg-4Y-3RE alloy. The material extruded at 573 K, followed by aging for 2 h, showed fine needle-like precipitates and the high density of a dislocation cell. This material exhibited a high strength of 370 MPa at room temperature. The material extruded at 673 K exhibited a very small grain size of 1.5 μm and fine spherical precipitates. This material showed not only a high strength of about 300 MPa from room temperature to 473 K, but also superplastic behavior at a high strain-rate of 4×10−1 s−1 and at 673 K. Furthermore, a good combination of high strength and high ductility at room temperature was attained for the material extruded at 673 K. These qualities can likely be attributed to the very small grain size.
  • Keywords
    Thermo-mechanical treatment , Mg-4Y-3RE , Hot extrusion , Artificial aging
  • Journal title
    MATERIALS SCIENCE & ENGINEERING: A
  • Serial Year
    1998
  • Journal title
    MATERIALS SCIENCE & ENGINEERING: A
  • Record number