Title of article :
Fabrication and characterization of TiC/Al composites
Author/Authors :
Hashimoto، نويسنده , , Shinobu and Yamaguchi، نويسنده , , Akira and Koshino، نويسنده , , Motoyuki، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 1999
Pages :
6
From page :
71
To page :
76
Abstract :
TiC/Al composites were fabricated by heating the powder mixture compacts consisting of Al and TiC in Ar. The effects of particle size of TiC as starting materials and cooling rate on microstructure of the composites were investigated. Further, the relationship between bending strength and microstructure of the composites was discussed. In case of heating the powder mixture compacts of 5:1 (mol ratio)=Al (10 μm): TiC (1–3 μm) at 1000–1500°C for 1 h, they became 95–97% in relative density. When the powder mixture compact was heated at 1100°C for 1 h and cooled to room temperature at a rate of 2°C/min, threadlike parts at which Al concentrated were formed in the compact. Then the average bending strength of the compact decreased to 270 from 400 MPa of the compact without Al concentrate parts, that was obtained by rapid cooling after the heating.
Keywords :
TiC/Al composites , microstructure , Bending strength , Powder mixture compacts
Journal title :
MATERIALS SCIENCE & ENGINEERING: A
Serial Year :
1999
Journal title :
MATERIALS SCIENCE & ENGINEERING: A
Record number :
2138585
Link To Document :
بازگشت