Title of article :
Effect of PWHT cycles on fatigue crack growth and toughness of quenched and tempered pressure vessel steels
Author/Authors :
Z. Sterjovski، نويسنده , , Z. and Carr، نويسنده , , D.G. and Dunne، نويسنده , , D.P. and Ambrose، نويسنده , , S.، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2005
Pages :
8
From page :
256
To page :
263
Abstract :
Transportable pressure vessels, commonly manufactured from quenched and tempered (QT) steels, require mandatory postweld heat treatment (PWHT) regardless of plate thickness. During their life, transportable pressure vessels may have up to 4 PWHT cycles at temperatures between 540 and 590 °C, and concerns have emerged about possible effects on the mechanical properties of the base (parent) plate. aper reports work on the resistance to fatigue crack growth, impact toughness and CTOD fracture toughness of two types of QT steels. The parent metal region was examined for both steels, and then exposed to temperatures and times in the PWHT range. Although there was a marginal decrease in the resistance to fatigue crack growth for up to four postweld heat treatment cycles, there was a significant decrease in impact toughness and CTOD fracture toughness.
Keywords :
Postweld heat treatment , CTOD , Void coalescence , impact toughness , Transportable pressure vessels , Fatigue crack growth , quenched and tempered steel