Texture development in Ti–6Al–4V linear friction welds
Author/Authors :
Karadge، نويسنده , , M. and Preuss، نويسنده , , M. and Lovell، نويسنده , , C. and Withers، نويسنده , , P.J. and Bray، نويسنده , , S.، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2007
Abstract :
Microstructure and microtexture development in as-welded and post weld heat treated (PWHT) lab-scale (LS) and full-scale (FS) Ti–6Al–4V linear friction welds have been characterized using scanning electron microscopy and electron back-scatter diffraction (EBSD). The full-scale specimens exhibited a plastically affected zone (PAZ) about twice the size compared to lab-scale test welds. At the weld line a region of very fine martensitically formed microstructure was observed in both the LS and FS friction welds. EBSD texture scans across the weld line revealed a sharp texture variation in the PAZ. At the weld line a strong { 1 0 1 ¯ 0 } 〈 1 1 2 ¯ 0 〉 transverse texture for the as-welded and PWHTed condition was observed in both welds. Whereas the lab-scale linear friction welds displayed a dramatic change from almost random to strong transverse texture in the PAZ, the full-scale linear friction welds exhibited transverse texture at the weld line, followed by dispersed bands of transverse and { 1 1 2 ¯ 2 } 〈 1 1 2 ¯ 3 〉 type rolling texture in the PAZ region. The observed difference in LS and FS weld region textures is attributed to a difference in the variant selections during β → α transformation.
Keywords :
Deformation , Texture , Linear friction welding , EBSD , Ti–6Al–4V
Journal title :
MATERIALS SCIENCE & ENGINEERING: A
Journal title :
MATERIALS SCIENCE & ENGINEERING: A