Title of article :
Thermal cycling response behavior of ceramic matrix composites under load and displacement constraints
Author/Authors :
Mei، نويسنده , , Hui and Cheng، نويسنده , , Laifei، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2008
Pages :
6
From page :
235
To page :
240
Abstract :
Thermal cycling response of a two-dimensional carbon fiber reinforced SiC matrix composite (2D C/SiC) to load constraint (LC) and to displacement constraint (DC) in an oxidizing environment was investigated. During thermal cycling between 700 and 1200 °C, a constraint strain with a 0.208% range and a constraint stress with a 180 MPa range were, respectively, generated on the composites in LC and DC. It was found that with increasing cycles, the constraint strain increased in LC and the constraint stress decreased in DC. After 50 cycles, in contrast to the as-received composite materials, the as-cycled composites suffered greater loss in mechanical properties: the residual strength and failure strain are 204 MPa and 0.49% for the LC tested samples, and 223 MPa and 0.64% for the DC tested samples, respectively. Microstructural observations indicated that the LC could develop thermal microcracks and assist in oxidizing the internal fibers, whereas the DC reduced crack propagations and fiber oxidation because of decreasing tensile and increasing compressive stresses.
Keywords :
microstructure , constraints , Ceramic matrix composites , Carbon fiber , thermal cycling
Journal title :
MATERIALS SCIENCE & ENGINEERING: A
Serial Year :
2008
Journal title :
MATERIALS SCIENCE & ENGINEERING: A
Record number :
2156133
Link To Document :
بازگشت