Title of article
Microstructure and microhardness of Ti6246 linear friction weld
Author/Authors
Guo، نويسنده , , Yina and Jung، نويسنده , , Taenam and Chiu، نويسنده , , Yu Lung and Li، نويسنده , , Hangyue and Bray، نويسنده , , Simon and Bowen، نويسنده , , Paul، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2013
Pages
8
From page
17
To page
24
Abstract
The microhardness and microstructure of linear friction welded Ti–6Al–2Sn–4Zr–6Mo (Ti6246) alloys were studied, in both as-welded and post-weld heat-treated conditions. It has been found that the as-welded Ti6246 has a lower microhardness value of about 360 HV in the central weld zone than that of the base material of about 420 HV. Post-weld heat-treatment of the Ti6246 weld at 600 °C for 1 h has led to the hardness increase of about 180 HV at the central weld zone. Transmission electron microscopy studies show that the microstructure at the central weld zone of the as-welded Ti6246 consists of fine grains with dense acicular orthorhombic α″ martensite. The soft α″ martensite is believed to account for the low hardness measured in the as-welded conditions. Phase transformation from orthorhombic α″ to hexagonal α occurred during the PWHT, resulting in the observed hardness increase.
Keywords
Linear friction welding , Titanium alloys , microstructure , Transmission electron microscopy
Journal title
MATERIALS SCIENCE & ENGINEERING: A
Serial Year
2013
Journal title
MATERIALS SCIENCE & ENGINEERING: A
Record number
2172312
Link To Document