Title of article :
Corrosion in water supply pipe stainless steel 304 and a supply line of helium in stainless steel 316
Author/Authors :
Martins، نويسنده , , C.M.B. and Moreira، نويسنده , , J.L. and Martins، نويسنده , , J.I.، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2014
Pages :
7
From page :
65
To page :
71
Abstract :
A corrosion spreading throughout the 304 stainless steel tubing of a water system to supply various buildings was observed, and also leaks were detected in welding zones. The same place is also crossed by a gas distribution network, with a helium pipe 316 of stainless steel that required periodic repairs more or less every two years, due to the presence of leaks. The tests showed that both types of stainless steel have suffered localized corrosion induced by hypochlorite ion, in a mechanism of dry/wet, and that the welding procedure performed on the 304 stainless steel is unacceptable. Some immediate procedures were undertaken to keep systems running, but recommendations were given for a final resolution of the problems.
Keywords :
Stainless steel 304 , Stainless steel 316 , Hypochlorite , Pitting corrosion , Welding
Journal title :
Engineering Failure Analysis
Serial Year :
2014
Journal title :
Engineering Failure Analysis
Record number :
2340020
Link To Document :
بازگشت