Title of article :
Shear Bond Strength of Orthodontic Attachments to Amalgam Surfaces Using Assure Universal Bonding Resin after Different Surface Treatments
Author/Authors :
Naseh ، Roya - Qazin University of Medical Sciences , Rahnamoon ، Nima - Lorestan University of Medical Sciences , Afshari ، Maryam - Qazvin University of Medical Sciences
Pages :
6
From page :
1
To page :
6
Abstract :
Background Assure Universal Bonding Resin is capable of providing a strong bond between orthodontic attachments and amalgam surfaces. Objectives This study sought to assess the shear bond strength of orthodontic attachments to amalgam surfaces using Assure Universal Bonding Resin after different surface treatments. Methods This invitro experimental study was conducted on 120 amalgam samples in eight groups of surface roughening with diamond bur, sandblasting with aluminum oxide particles, Er, Cr: YSGG laser irradiation and polishingonly. Molar buccal tubes were bonded to amalgam surfaces using Assure primer and Transbond Plus lightcure composite. Half the samples were immediately subjected to shear bond strength testing while the remaining half were incubated at 37°C for one week, thermocycled (1000 cycles) and were then subjected to shear bond strength test. Oneway ANOVA was applied to compare the bond strength of the groups and Tukey’s test was used for pairwise comparisons. The adhesive remnant index (ARI; 4 pointscale) was also determined in the groups and the results were analyzed using the KruskalWallis test. Results Significant differences were noted in shear bond strength of attachments following the application of Assure among different surface treatment modalities (P amp;lt; 0.001); the highest bond strength was noted in sandblasted group followed by laser, bur and polishing, respectively. Aging had no significant effect on bond strength. Conclusions Sandblasting and irradiation of Er, Cr: YSGG laser provided sufficiently high bond strength between amalgam and attachments following the application of Assure. Diamond bur and polishing did not provide adequately high bond strength.
Keywords :
Assure Universal Bonding Resin , Shear Bond Strength , Er , Cr: YSGG Laser , Sandblasting , Amalgam
Journal title :
Iranian Journal of Orthodontics
Serial Year :
2011
Journal title :
Iranian Journal of Orthodontics
Record number :
2440830
Link To Document :
بازگشت