Abstract
A theoretical model was developed that allows to predict the erosion mechanism of water insoluble biodegradable polymer matrices. The model shows that all degradable polymers can undergo surface erosion or bulk erosion. Which way a polymer matrix erodes after all depends on the diffusivity of water inside the matrix, the degradation rate of the polymerʹs functional groups and the matrix dimensions. From these parameters the model allows to calculate for an individual polymer matrix a dimensionless ‘erosion number’ . The value of indicates the mode of erosion. Based on , a critical device dimension Lcritical can be calculated. If a matrix is larger than Lcritical it will undergo surface erosion, if not it will be bulk eroding. Lcritical values for polymers were estimated based on literature data. Polyanhydrides were found to be surface eroding down to a size of approximately Lcritical=10−4 m while poly(α-hydroxy esters) matrices need to be larger than Lcritical=10−1 m to lose their bulk erosion properties. To support our theoretical findings it was shown experimentally that poly(α-hydroxy ester) matrices, which are considered classical bulk eroding materials, can also undergo surface erosion.
Keywords
PLGA , Bulk erosion , modeling , Surface erosion , PLA , degradation
Journal title
Biomaterials
Serial Year
2002
Journal title
Biomaterials
Record number
544538
Link To Document