Title of article
Interaction of limestone grains and acidic solutions from the oxidation of pyrite tailings
Author/Authors
M. Sim?n، نويسنده , , F. Mart?n، نويسنده , , I. Garc?a، نويسنده , , P. Bouza، نويسنده , , C. Dorronsoro، نويسنده , , J. Aguilar، نويسنده ,
Issue Information
روزنامه با شماره پیاپی سال 2005
Pages
8
From page
65
To page
72
Abstract
To characterise the coatings formed and to analyse element partitioning between the aqueous and solid phase, suspensions were prepared with four grain sizes of limestone and three different amounts of acidic solution from oxidized pyrite tailings. In all cases, red coatings with three different layers covered the grain surface, sealing off the acidic solution. The inner layer was composed mainly of basaluminite, the middle layer of schwertmannite, and the outer layer of gypsum and jarosite. Zn, Cd and Tl were co-precipitated by Fe and Al; As and Pb were co-precipitated almost completely by Fe; and Cu formed mainly Cu sulphates. All trace elements reached almost total precipitation at pH 6.3, but the precipitation of As and Pb tended to decrease as the pH rose. Consequently, liming should be calculated so that the soil pH does not exceed 6.3. This calculation should take into account that the armouring of the limestone grains can cause underestimations in the amount of liming material needed.
Keywords
Coatings , pollutants , Limestone , Tailings oxidation , Element precipitation