Author/Authors :
S. Maitra، نويسنده , , A. CHOUDHURY، نويسنده , , H. S. DAS، نويسنده , , MS. J. PRAMANIK، نويسنده ,
Abstract :
Many workers [1–9] studied the kinetics of dolomite decomposition to study the effects of
different parameters like, gas (CO2, N2 etc.) pressures, water vapor, presence of other
impurities, particle size and grain size of the dolomite samples, crystallinity etc. on the
decomposition kinetics of dolomite using different tools like, thermal analysis,
thermo-gravimetric analyses, XRD technique etc. and different values of the activation
energies for the decomposition reaction, order of reactions have been reported. It has been
observed that pure dolomite decomposed in only two steps. The first stage of the thermal
decomposition of dolomite resulted in the formation of Mg-calcite [(CaMg)CO3] and
periclase (MgO), with the liberation of CO2. It was further observed that under CO2,
dolomite decomposed directly to CaCO3, accompanied by the formation of MgO between
550 and 765◦C. Calcite decomposed to CaO between 900 and 960◦C and under air,
simultaneous formation of CaCO3, CaO and MgO accompanied dolomite decomposition
between 700 and 740–750◦C. At the latter temperature, the calcite began to decompose
even though a significant amount of dolomite was still present and simultaneous
decomposition of the two carbonates was terminated at 780◦C. Also, changes in
decomposition rates of the various phases correlated with changes in the rate of weight
loss determined by derivative thermo-gravimetric analysis.