Hydrothermal corrosion behavior of iron aluminide under SCWO conditions
Author/Authors :
V. Shankar Rao، نويسنده , , H. S. Kwon، نويسنده ,
Issue Information :
دوهفته نامه با شماره پیاپی سال 2007
Pages :
5
From page :
4530
To page :
4534
Abstract :
Fe3Al based iron aluminide was tested under supercritical water oxidation (SCWO) conditions to explore its possible use as a reactor material for hydrothermal processes. Degradation resistance of the material were evaluated in distilled water at 450 C and 300 atm in a closed reactor. The results of the kinetics studies, metallographic observations as well as phase and chemical analysis of the corrosion products indicated limited applicability of iron aluminide in SCWO conditions