Abstract :
Zr-doped TiO2 (anatase) was prepared by the
homogenous co-precipitation method of the aqueous solutions
containing TiOSO4 and ZrCl4 using urea as the precipitation
agent. Nanocrystallites of Zr-doped TiO2,
6–9 nm in size, intergrown with amorphous phase form
1–2 lm porous spherical clusters. Crystallite size of anatase
decreases with increasing Zr content, and the catalyst
becomes totally amorphous at 10 mol.% Zr. All samples
exhibit high specific surface area, which increases with the
addition of zirconium (from 391.3 to 689.1 m2 g–1).