Author/Authors :
Haijun Ma، نويسنده , , Yajiang Li، نويسنده , , S. A. Gerasimov، نويسنده , ,
Juan Wang، نويسنده ,
Abstract :
Three different Cr–Ni alloys were deposited on
the surface of Fe3Al intermetallic by shielded metal arc
welding (SMAW) to investigate the weldability of this
material. The microstructure, phase constitutions, and fine
structures of Cr–Ni surfacing layers were analyzed via
metalloscope, SEM, XRD, and TEM. The results indicated
that the Fe3Al/Cr–Ni joint shows no cracks when Cr25–
Ni13 alloy was deposited. The surfacing layer consisted of
austenite (A), pro-eutectoid ferrite (PF), carbide-free bainite
(CFB), lath martensite (LM), and little acicular ferrite
(AF). Phase constitutions of the joint included Fe3Al, FeAl,
c-(Fe,C), c-(Fe,Ni), NiAl, and Ni3Al. The lattice orientation
for CFB between a and c phases was (110)a//(111)c.
Typical LM was composed of interlayer-carbide and a
ferrite of 400 nm in length and 40 nm in width