Author/Authors :
S. M. H. Mirbagheri، نويسنده , , S. Sookhtehsaraee، نويسنده ,
Abstract :
In the present study, a novel procedure was
introduced for casting of metal matrix composites by
adding a mortar consisting expandable polystyrene beads,
carboxy methyl cellulose paste, SiC particles and water as
a mould pattern. This process was applied for A356 Aluminium
alloy/SiCP composite. Technology of this method
is based on a balance between the solidification rate and the
buoyancy of the reinforcement particles. The experimental
results show that effective parameters in fabrication of a
sound part are density and size of pre-puff polystyrene
beads, percentage of the reinforcement particles, mould
material, thickness of mould cavity, casting temperature
and cooling rate. However, the innovative method will only
be successful for the thin-wall parts, which their solidification
times become shorter than the floatation time of the
reinforcement particles