• DocumentCode
    1029173
  • Title

    Very low core loss high silicon-iron ribbons

  • Author

    Arai, K.I. ; Ohmori, K. ; Satoh, T. ; Yamashiro, Y. ; Satoh, T. ; Yamashiro, Y.

  • Author_Institution
    Tohoku University, Sendai, Japan
  • Volume
    23
  • Issue
    5
  • fYear
    1987
  • fDate
    9/1/1987 12:00:00 AM
  • Firstpage
    3221
  • Lastpage
    3226
  • Abstract
    Rapidly quenched 4.5wt% silicon-iron ribbons 280/μm thick were cold-rolled with large thickness reduction in each rolling pass for a total thickness reduction of 70% or more. After annealing at high temperatures in a vacuum, they had highly oriented
  • Keywords
    Annealing; Core loss; Grain size; Temperature dependence;
  • fLanguage
    English
  • Journal_Title
    Magnetics, IEEE Transactions on
  • Publisher
    ieee
  • ISSN
    0018-9464
  • Type

    jour

  • DOI
    10.1109/TMAG.1987.1065472