Abstract :
A number of silicone rubber composite insulators have been examined following 15 years of service on a coastal 400 kV transmission line in the UK. Extensive measurements of their hydrophobicity, as determined by contact angle, are given along with a description of their appearance. The hydrophobicity change varied from the low voltage end to the high voltage end with the lowest contact angles being found in the middle of the string. The sheds also aged differently around their circumference and this was reflected in discoloration differences on different sides of the insulator, in addition to hydrophobicity changes. The greatest change to properties was witnessed on the core of the insulators on which contact angles of less than 70 degrees were recorded
Keywords :
ageing; composite insulators; power transmission lines; silicone rubber insulators; 400 kV; UK; composite insulators; hydrophobicity measurement; power transmission lines; silicone rubber aging; Aging; Ceramics; Dielectrics and electrical insulation; Flashover; Low voltage; Plastic insulation; Polymers; Rubber; Stress; Transmission lines;
fLanguage :
English
Journal_Title :
Dielectrics and Electrical Insulation, IEEE Transactions on
Publisher :
ieee
ISSN :
1070-9878
Type :
jour
DOI :
10.1109/TDEI.2007.302881
Filename :
4088920
Link To Document :
بازگشت