DocumentCode :
1259195
Title :
(110) grain growth and magnetic properties of thin grain-oriented 3% silicon steel sheets
Author :
Nanako, M. ; Fukunaga, Hirotoshi ; Ishiyama, Kaznshi ; Arai, Kenichi
Author_Institution :
Nagasaki Univ., Japan
Volume :
35
Issue :
5
fYear :
1999
fDate :
9/1/1999 12:00:00 AM
Firstpage :
3379
Lastpage :
3381
Abstract :
(110) grain growth and magnetic properties in thin grain-oriented silicon sheets with ultimately low loss were investigated. A final-annealing at 1150°C for 20 min enables us to obtain the thin sheets covered with only (110) grains and consequently the magnetic induction at 800 A/m, Bg reached 1.9 T
Keywords :
annealing; electromagnetic induction; ferromagnetic materials; grain growth; iron alloys; magnetic leakage; silicon alloys; (110) grain growth; 1150 degC; Fe-Si; final-annealing; low loss; magnetic induction; magnetic properties; thin grain-oriented 3% silicon steel sheets; Annealing; Coercive force; Grain boundaries; Inhibitors; Iron; Magnetic properties; Production; Silicon; Steel; Temperature;
fLanguage :
English
Journal_Title :
Magnetics, IEEE Transactions on
Publisher :
ieee
ISSN :
0018-9464
Type :
jour
DOI :
10.1109/20.800530
Filename :
800530
Link To Document :
بازگشت