Abstract :
Gilbert´s damping constants, α , of Co-Cr-Ta and Co-Cr-Pt thin films are determined by Q-band FMR analysis using single crystal magnetic thin films epitaxialIy grown on MgO(110) substrates. α is calculated from the resonance width of the FMR spectrum. α of Co77Cr19Ta4 is found to increase from 0.016 to 0.028 as magnetic layer thickness increases from 25 to 240 nm. α also increases from 0.009 to 0.019 when the Cr concentration in the 60 nm thick Co96-x CrxTa4 magnetic layer is increased from 8 to 19 at.%. The 25 nm thick Co81Cr15Pt4, film has a 2.5 times larger α value (0.038) than the Co81Cr15Ta4 film (α = 0.014) with the same thickness.
Keywords :
chromium alloys; cobalt alloys; damping; ferromagnetic resonance; magnetic epitaxial layers; platinum alloys; tantalum alloys; Co-Cr-Pt; Co-Cr-Ta; Gilbert damping constant; Q-band FMR; epitaxial growth; single crystal magnetic thin film; Chromium; Damping; Magnetic analysis; Magnetic films; Magnetic resonance; Substrates; Transistors;
fLanguage :
English
Journal_Title :
Magnetics, IEEE Transactions on
Publisher :
ieee
ISSN :
0018-9464
Type :
jour
DOI :
10.1109/20.617820
Filename :
617820
Link To Document :
بازگشت