• DocumentCode
    1984602
  • Title

    RTV silicone rubber hydrophobicity loss and recovery character under AC corona

  • Author

    Dai, Rijun ; Wang, Shenghui ; Lu, Fangcheng

  • Author_Institution
    Inner Mongolia GuoDian Energy Investment Co. Ltd., Hohhot, China
  • fYear
    2011
  • fDate
    16-18 Sept. 2011
  • Firstpage
    807
  • Lastpage
    810
  • Abstract
    In this paper, the effect of AC Corona on the hydrophobicity of room temperature vulcanizing (RTV) silicone rubber materials is studied with a pin-plate electrode corona accelerate aging model. Experiments show that AC corona can make the RTV specimen hydrophobicity lose rapidly, further, the hydrophobicity recovery character of RTV specimen is also researched through a long time of corona test, as a result, it is found that the RTV specimen hydrophobicity recovery speed is not continuous, but having an alternate process of "speed up" and "slow down". After corona time reaches a certain time, the hydrophobicity recovery time dramatically becomes longer but it still can not fully restore to the initial value in the end. meanwhile research find that when the corona time is in a certain range, after the hydrophobicity recovery, the final static contact angle is much larger than the initial value before the corona.
  • Keywords
    corona; hydrophobicity; silicone rubber insulators; AC corona; RTV silicone rubber hydrophobicity loss; aging model; pin-plate electrode corona; room temperature vulcanizing rubber materials; Chemicals; Corona; Discharges; Materials; Rubber; Surface discharges; Surface treatment; Aging; RTV (room temperature vulcanizing) silicone rubber; corona; hydrophobicity; static contact angle;
  • fLanguage
    English
  • Publisher
    ieee
  • Conference_Titel
    Electrical and Control Engineering (ICECE), 2011 International Conference on
  • Conference_Location
    Yichang
  • Print_ISBN
    978-1-4244-8162-0
  • Type

    conf

  • DOI
    10.1109/ICECENG.2011.6057582
  • Filename
    6057582